Polymer Property : Deflection Temperature at 1.8 MPa (264 psi) = 435 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 435 °C
815 °F
ASTM D648
PBI Performance Products Celazole® PBI U-60 Unfilled Polybenzimidazole Resin
U-60 grade Celazole® polybenzimidazole (PBI) resin is a organic polymer which does not burn in air and has high temperature resistance, along with excellent stability to chemicals and hydrolysis. ..