Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 256 °C | 492 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PA6/6 E GF33 LE 33% Mineral Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightFeatures: Low ExtractablesProcessing Method: ExtrusionInformation provided by TP Composi.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 256 °C | 492 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PA6/6 GF30 HR L 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Heat Stabilized, Lubricated and Hydroly.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 256 °C | 492 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PA6/6 GF33 HR L 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: LubricantFeatures: Lubricated and Hydrolysis Resistant TPCI# 9357101Informatio.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 256 °C | 492 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PA6/6 GF33 HS L BK 33% Glass Filled (Dry) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedAppearanc.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 256 °C | 492 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PA6/6 GF33 L BKN001 33% Glass Filled (Dry) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedAppearanc.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 256 °C | 492 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PA6/6 GF33 NAT001 Y 33% Glass Filled (Dry) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedUL File N.. |