Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 51.9 °C | 125 °F | ASTM D648-98c |
DSM Somos® ProtoTherm™ 12120 Water-resistant resin for stereolithography, UV Postcure DescriptionDSM Somos® 12120 is a liquid photopolymer that produces strong, high temperature tolerant, water-resistant parts. Parts created with Somos® 12120 have a cherry-red appearance which tur.. |