Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 53.3 °C
128 °F
ASTM D648
RheTech Products FT7013-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural
Applications: Scuff platesLift gate coversI/P componentsClose-out panelsInjection molding conditions reported in table.Information provided by RheTech Products.
Deflection Temperature at 1.8 MPa (264 psi) 53.3 °C
128 °F
ASTM D648
RheTech Products FT7013-720UV Thermoplastic Polyolefin, UV Stabilized, XTM Dark Sandstone
Applications: Scuff platesLift gate coversI/P componentsClose-out panelsInjection molding conditions reported in table.Information provided by RheTech Products.
Deflection Temperature at 1.8 MPa (264 psi) 53.3 °C
128 °F
ASTM D648
RheTech Products FT7013-721UV Thermoplastic Polyolefin, UV Stabilized, XDV Dark Slate
Applications: Scuff platesLift gate coversI/P componentsClose-out panelsInjection molding conditions reported in table.Information provided by RheTech Products.
Deflection Temperature at 1.8 MPa (264 psi) 53.3 °C
128 °F
ASTM D648
RheTech Products FT7016-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural
Applications: Bumper coversCladdingsInjection molding conditions reported in table.Information provided by RheTech Products.
Deflection Temperature at 1.8 MPa (264 psi) 53.3 °C
128 °F
ASTM D648
RheTech Products FT7016-01 Thermoplastic Polyolefin, Non-UV Stabilized, Black
Applications: Bumper coversCladdingsInjection molding conditions reported in table.Information provided by RheTech Products.
Deflection Temperature at 1.8 MPa (264 psi) 53.3 °C
128 °F
ASTM D648
RheTech Products FT7016-01UV Thermoplastic Polyolefin, UV Stabilized, Black
Applications: Bumper coversCladdingsInjection molding conditions reported in table.Information provided by RheTech Products.
Deflection Temperature at 1.8 MPa (264 psi) 53.3 °C
128 °F
ASTM D648
RheTech Products FT7016-50UV Thermoplastic Polyolefin, UV Stabilized, YGYA Black
Applications: Bumper coversCladdingsInjection molding conditions reported in table.Information provided by RheTech Products.
Deflection Temperature at 1.8 MPa (264 psi) 53.3 °C
128 °F
ASTM D648-98c
DSM Somos® ProtoGen™ 18920 Liquid Photopolymer, UV Postcure at HOC +3
Product DescriptionDSM Somos® ProtoGen 18920 is a liquid photopolymer that produces accurate, ABS-like parts ideal for general purpose applications. ProtoGen resins are the first SL resins to demo..
Deflection Temperature at 1.8 MPa (264 psi) 53.3 °C
128 °F
ISO 75-2/A
ExxonMobil AP3AW Polypropylene Impact Copolymer
Product Description: A UV stabilized medium impact copolymer resin designed for automotive battery cases.Availability: Asia Pacific Features:Good UV ResistanceHigh StiffnessLow WarpageMedium FlowMe..
Deflection Temperature at 1.8 MPa (264 psi) 53.3 °C
128 °F
Aclo Accutech Polypropylene Homopolymer HP0339G15M15CL Glass/Mineral Reinforced Coupled
Deflection Temperature at 1.8 MPa (264 psi) 53.3 °C
128 °F
BCC Products BC 7020 Epoxy Backfill System
BC 7020 is a lightweight two component epoxy backfill system. Unlike BC 7010, the filler portion is pre-blended into the resin and hardener components for easier handling, thus simplifying the mixin..