Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 281 °C
538 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
SABIC Innovative Plastics LNP LUBRICOMP 9X98026 PA 46 (Europe-Africa-Middle East)
LNP* Lubricomp* 9X98026 is a compound based on PA4.6 resin containing Barium Sulfate, PTFE and Carbon Fiber
Deflection Temperature at 1.8 MPa (264 psi) 281 °C
538 °F
Unannealed; ASTM D648
Solvay Specialty Polymers Torlon® 4645 Polyamide-imide (PAI)  (Unverified Data**)
Torlon 4645, an injection-moldable, wear-resistant grade of polyamide-imide (PAI), has been formulated to give outstanding wear resistance in lubricated wear applications. Torlon PAI has the highest..
Deflection Temperature at 1.8 MPa (264 psi) 281 °C
538 °F
Unannealed; ISO 75-2/A
Solvay Specialty Polymers Amodel® A-1145 HS Polyphthalamide (PPA), 45% Glass Fiber (Dry)
Amodel® A-1145 HS is a 45% glass reinforced, heat stabilized polyphthalamide (PPA) with a high heat deflection temperature, very high flexural modulus and very high tensile strength. Excellent cr..
Deflection Temperature at 1.8 MPa (264 psi) 281 °C
538 °F
Unannealed; ASTM D648
Solvay Specialty Polymers Torlon® 4645 Polyamide-imide (PAI)
Torlon® 4645, an injection-moldable, wear-resistant grade of polyamide-imide (PAI), has been formulated to give outstanding wear resistance in lubricated wear applications.Features: Flame Retarda..
Deflection Temperature at 1.8 MPa (264 psi) 281 °C

@Thickness 3.20 mm
538 °F

@Thickness 0.126 in
unannealed; ASTM D648
SABIC Innovative Plastics LNP THERMOCOMP UF0067W PPA
LNP* THERMOCOMP* UF0067W is a compound based on Polyphthalamide resin containing 30% glass fiber. Added features of this material include: Hot Water Moldable, Non-Brominated & Non-Chlorinated Flam..
Deflection Temperature at 1.8 MPa (264 psi) 281 °C

@Thickness 3.20 mm
538 °F

@Thickness 0.126 in
unannealed; ASTM D648
SABIC Innovative Plastics LNP THERMOCOMP UF008H PPA
LNP THERMOCOMP* UF008H is a compound based on Polyphthalamide resin containing 40% Glass Fiber. Added feature of this grade is: Healthcare.
Deflection Temperature at 1.8 MPa (264 psi) 281 °C
538 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
SABIC Innovative Plastics LNP THERMOCOMP UF00ASW PPA
LNP* Thermocomp* UF00ASW is a compound based on Polyphthalamide (PPA) containing glass fiber. Characteristics of this grade of Heat Stabilized and Hot Water Moldable.
Deflection Temperature at 1.8 MPa (264 psi) 281 °C

@Thickness 3.20 mm
538 °F

@Thickness 0.126 in
unannealed; ASTM D648
SABIC Innovative Plastics LNP THERMOCOMP UF008H PPA (Asia Pacific)
LNP THERMOCOMP* UF008H is a compound based on Polyphthalamide resin containing Glass Fiber.
Deflection Temperature at 1.8 MPa (264 psi) 281 °C
538 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
SABIC Innovative Plastics LNP Verton OV00A PPS (Asia Pacific)
LNP* Verton* OV00A is a compound based on Polyphenylene Sulfide resin containing Long Glass Fiber.This data was supplied by SABIC-IP for the Asia Pacific region.
Deflection Temperature at 1.8 MPa (264 psi) 281 °C
538 °F
DAM; ISO 75-1/-2
DuPont Performance Polymers Zytel® HTN FR52G30NHF BK337 Polyphthalamide (PPA)
30% Glass Reinforced Flame Retardant Non-Halogenated PPA High Performance Polyamide with Improved Flow Zytel HTNFR52G30NHF BK337 is a 30% glass reinforced flame retardant lubricated high performance..
Deflection Temperature at 1.8 MPa (264 psi) 281 °C
538 °F
DAM; ISO 75-1/-2
DuPont Performance Polymers Zytel® HTN FR52G30NHF BK337 Polyphthalamide (PPA)  (Unverified Data**)
Zytel® HTNFR52G30NHF BK337 is a 30% glass reinforced, flame retardant, lubricated high performance polyamide resin with improved flow. It is also a PPA resin and it uses a non-halogenated flame ret..
Deflection Temperature at 1.8 MPa (264 psi) 281 °C
538 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
SABIC Innovative Plastics LNP Verton OV00A PPS
LNP* Verton* OV00A is a compound based on Polyphenylene Sulfide resin containing Long Glass Fiber.This data was supplied by SABIC-IP for the Americas region.