Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 54.44 °C | 130.0 °F | ASTM D648 |
Lucent Polymers CPP-0307 Polypropylene, Mineral Filled, Impact Modified Recycled ContentAdd "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 54.44 °C | 130.0 °F | ASTM D648 |
Lucent Polymers CPP-310 Polypropylene, 10% Calcium Carbonate Filled, Impact Modified Melt Flow Adjustable for ApplicationAdd "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 54.44 °C | 130.0 °F | ASTM D648 |
Lucent Polymers TPP-310 Polypropylene, 10% Talc Filled, Impact Modified Melt Flow Adjustable for ApplicationAdd "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 54.44 °C | 130.0 °F | ASTM D648 |
Lucent Polymers PPH-110 Polypropylene, Homopolymer Add "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc. |