Deflection Temperature at 1.8 MPa (264 psi) 286 °C
547 °F
Unannealed; ASTM D648
LNP Thermocomp® UC-1006 Polyphthalamide, Carbon Fiber Reinforcement  (discontinued **)
Forms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still active under new names..
Deflection Temperature at 1.8 MPa (264 psi) 286 °C

@Thickness 3.20 mm
547 °F

@Thickness 0.126 in
unannealed; ASTM D648
SABIC Innovative Plastics LNP THERMOCOMP LF004E PEEK (Asia Pacific)