Deflection Temperature at 1.8 MPa (264 psi) 291 °C
556 °F
Unannealed; ASTM D648
Solvay Specialty Polymers KetaSpire® KT-820 SL30 Polyetheretherketone (PEEK)  (Unverified Data**)
Ketaspire KT-820 SL30 is a polyetheretherketone (PEEK) compound designed to provide a balance of excellent mechanical properties, wear resistance and low coefficient of friction in both dry and exte..
Deflection Temperature at 1.8 MPa (264 psi) 291 °C
556 °F
Annealed; ASTM D648
Solvay Specialty Polymers KetaSpire® KT-820 SL30 Polyetheretherketone (PEEK)  (Unverified Data**)
Ketaspire KT-820 SL30 is a polyetheretherketone (PEEK) compound designed to provide a balance of excellent mechanical properties, wear resistance and low coefficient of friction in both dry and exte..
Deflection Temperature at 1.8 MPa (264 psi) 291 °C

@Thickness 3.20 mm
556 °F

@Thickness 0.126 in
Annealed; ASTM D648
Solvay Specialty Polymers Amodel® A-6135 HN Polyphthalamide (PPA), 35% Glass Fiber (Dry)
Amodel® A-6135 HN polyphthalamide (PPA) is a 35% glass reinforced resin that is heat stabilized, lubricated and hot-water moldable. Key properties of the resin are high heat resistance, high stre..
Deflection Temperature at 1.8 MPa (264 psi) 291 °C
556 °F
Unannealed; ASTM D648
Solvay Specialty Polymers KetaSpire® KT-820 SL30 Polyetheretherketone (PEEK)
KetaSpire® KT-820 SL30 is a polyetheretherketone (PEEK) compound designed to provide a balance of excellent mechanical properties, wear resistance and low coefficient of friction in both dry and ..
Deflection Temperature at 1.8 MPa (264 psi) 291 °C
556 °F
Annealed; ASTM D648
Solvay Specialty Polymers KetaSpire® KT-820 SL30 Polyetheretherketone (PEEK)
KetaSpire® KT-820 SL30 is a polyetheretherketone (PEEK) compound designed to provide a balance of excellent mechanical properties, wear resistance and low coefficient of friction in both dry and ..
Deflection Temperature at 1.8 MPa (264 psi) 291 °C

@Thickness 3.20 mm
556 °F

@Thickness 0.126 in
Annealed; ASTM D648
Solvay Specialty Polymers Amodel® A-6135 HN Polyphthalamide (PPA)  (Unverified Data**)
Amodel A-6135 HN polyphthalamide (PPA) is a 35% glass reinforced resin that is heat stabilized, lubricated and hot-water moldable. Key properties of the resin are high heat resistance, high strength..