Polymer Property : Deflection Temperature at 1.8 MPa (264 psi) = 62.78 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 62.78 °C
145.0 °F
ASTM D648
Lucent Polymers CPP-120 Polypropylene Homopolymer, 20% Calcium Carbonate Filled
Melt Flow Adjustable for ApplicationAdd "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc.
Deflection Temperature at 1.8 MPa (264 psi) 62.78 °C
145.0 °F
ASTM D648
Lucent Polymers CPP-330 Polypropylene, 30% Calcium Carbonate Filled, Impact Modified
Melt Flow Adjustable for ApplicationAdd "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc.
Deflection Temperature at 1.8 MPa (264 psi) 62.78 °C
145.0 °F
ASTM D648
Lucent Polymers CPP-340 Polypropylene, 40% Calcium Carbonate Filled, Impact Modified
Melt Flow Adjustable for ApplicationAdd "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc.