Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 69.00 °C
156.2 °F
annealed; ASTM D-648
Axiall CL-6400 Rigid PVC, Molding
Georgia Gulf CL-6400 is a high flow clear PVC compound designed for thin wall parts and multi-cavity molds. It is ideally suited for a variety of electrical and appliance applications.Information p..
Deflection Temperature at 1.8 MPa (264 psi) 69.00 °C
156.2 °F
annealed; ASTM D-648
Axiall SP-6655 Rigid PVC, Molding
Georgia Gulf SP-6655 is a high flow rigid PVC compound designed for electrical and custom molding applications. This compound features excellent physical properties, good melt flow, and exceptional..
Deflection Temperature at 1.8 MPa (264 psi) 69.00 °C
156.2 °F
annealed; ASTM D-648
Axiall SP-6235 Rigid PVC, Molding
Georgia Gulf SP-6235 is a high flow rigid PVC compound designed for electrical and custom molding applications. This compound features excellent physical properties, high melt flow and exceptionall..