Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 72.00 °C
161.6 °F
ASTM D-648
Axiall LR-5009 Rigid PVC, Molding, All Colors
Georgia Gulf LR-5009 is an economical high flow rigid PVC fittings compound designed for multi-cavity molds and large diameter fittings. This compound is characterized by excellent process ability,..