Polymer Property : Deflection Temperature at 1.8 MPa (264 psi) = 76.6 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 76.6 °C
170 °F
Annealed; ASTM D648
PolyOne Geon™ Vinyl Rigid Extrusion L4536 Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne
Deflection Temperature at 1.8 MPa (264 psi) 76.6 °C
170 °F
Annealed; ASTM D648
PolyOne Geon™ Vinyl Rigid Extrusion LR620 white 1046 Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne