Deflection Temperature at 1.8 MPa (264 psi) 46.7 - 87.2 °C
116 - 189 °F
Average value: 70.7 °C Grade Count:43
Overview of materials for PVC, Molded
This property data is a summary of similar materials in the MatWeb database for the category "PVC, Molded". Each property range of values reported is minimum and maximum values of appropriate MatWeb..