Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 88.3 °C @Thickness 6.35 mm |
191 °F @Thickness 0.250 in |
Unannealed; ASTM D648 |
PolyOne Edgetek® XT XT-500-CU00 Polycarbonate + PBT (PC+PBT) EDGETEK™ XT High Performance Polymers are polycarbonate and polyester alloys that combine strength, durability and chemical resistance. The Edgetek XT product family includes a complete line of gen.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 88.3 °C @Thickness 6.35 mm |
191 °F @Thickness 0.250 in |
Annealed; ASTM D648 |
PolyOne Edgetek® XT XT-500-CX02 PC+PBT
(discontinued **) EDGETEK™ XT High Performance Polymers are polycarbonate and polyester alloys that combine strength, durability and chemical resistance. The Edgetek XT product family includes a complete line of gen.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 88.3 °C | 191 °F | Annealed; ASTM D648 |
American Polymers API 500 Polystyrene API 500 is a heat resistant grade of impact polystyrene. It has superior heat resistance, good impact resistance and easy colorability.Applications: API 500 is used in housewares, toys, containers,.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 88.3 °C | 191 °F | 0.125 in bar Unannealed/Conditioned 48 hours at 23°C; ASTM D648 |
Diamond Polymers ABS 4001HH Description: Heat Resistant Grade, High HeatInformation provided by Diamond Polymers, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 88.3 °C | 191 °F | Unannealed; ASTM D648 |
Entec Hyrene® PSCRY 2.5 General Purpose Polystyrene Available in North America Features: Crystal, General Purpose, and High Heat ResistanceRoHS Compliant Form: Pellets Information provided by Entec |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 88.3 °C | 191 °F | ASTM D-648 |
Axiall HHW-191 Rigid PVC, Extrusion Georgia Gulf HHW-191 is a special purpose profile extrusion alloy designed for applications requiring the following properties: Excellent WeatherabilityImpact Strength & ToughnessColorabilityChemic.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 88.3 °C | 191 °F | ASTM D648 |
Americas Styrenics MB3150 High Heat Crystal Polystyrene Product CharacteristicsFast cycling due to high heat distortion temperatureHigh vicat softening temperatureExcellent clarity with slight blue tintGood toughnessFood Contact CompliantUL Classificatio.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 88.3 °C | 191 °F | ASTM D648 |
Americas Styrenics STYRON® 610 High Heat Crystal Polystyrene Product CharacteristicsAdditive freeTypical ApplicationsFoamsFilms/opticalCarrier resinSpecialty blendingInformation provided by AmericasStyrenics LLC. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 88.3 °C @Thickness 6.35 mm |
191 °F @Thickness 0.250 in |
Annealed; ASTM D648 |
PolyOne Edgetek® XT XT-500-CX00 PC+PBT
(discontinued **) EDGETEK™ XT High Performance Polymers are polycarbonate and polyester alloys that combine strength, durability and chemical resistance. The Edgetek XT product family includes a complete line of gen.. |