Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 32.0 - 34.0 °C
89.6 - 93.2 °F
ASTM D648-07
Proto3000 Objet DurusWhite FullCure430 Polypropylene-like Prototyping Polymer
Objet’s FullCure® Materials family of proprietary acrylic-based photopolymer materials enables Objet users to create highly accurate, finely detailed 3D models and parts for a wide range of Rapid ..
Deflection Temperature at 1.8 MPa (264 psi) 32.0 °C

@Thickness 3.20 mm
89.6 °F

@Thickness 0.126 in
unannealed; ASTM D648
SABIC Innovative Plastics LNP LUBRICOMP LCL33EXQ PEEK
LNP* LUBRICOMP* LCL33EXQ is a compound based on Polyetheretherketone containing 15% Carbon Fiber, 15% PTFE. Added features of this material include: Wear Resistant, Easy Molding.