Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 98.3 °C

@Thickness 6.35 mm
209 °F

@Thickness 0.250 in
Unannealed; ASTM D648
PolyOne Edgetek® XT XT-100-BU01-HF Polycarbonate + PBT (PC+PBT)
EDGETEK™ XT High Performance Polymers are polycarbonate and polyester alloys that combine strength, durability and chemical resistance. The Edgetek XT product family includes a complete line of gen..
Deflection Temperature at 1.8 MPa (264 psi) 98.3 °C
209 °F
ASTM D648
Polymer Resources ABS-G15 ABS, 15% Glass Reinforced
Acrylonitrile Butadiene Styrene, 15% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information..
Deflection Temperature at 1.8 MPa (264 psi) 98.3 °C
209 °F
0.125 in bar Unannealed/Conditioned 48 hours at 23°C; ASTM D648
Diamond Polymers ASA/PC TA-35
Description: ASA Weatherable Polymer, Injection Molding Grade, Very High ImpactInformation provided by Diamond Polymers, Inc.
Deflection Temperature at 1.8 MPa (264 psi) 98.3 °C

@Thickness 6.35 mm
209 °F

@Thickness 0.250 in
Annealed; ASTM D648
PolyOne Edgetek® XT XT-100-CX00 PC+PBT  (discontinued **)
EDGETEK™ XT High Performance Polymers are polycarbonate and polyester alloys that combine strength, durability and chemical resistance. The Edgetek XT product family includes a complete line of gen..
Deflection Temperature at 1.8 MPa (264 psi) 98.3 °C

@Thickness 6.35 mm
209 °F

@Thickness 0.250 in
Annealed; ASTM D648
PolyOne Edgetek® XT XT-100-CX02-EG PC+PBT  (discontinued **)
EDGETEK™ XT High Performance Polymers are polycarbonate and polyester alloys that combine strength, durability and chemical resistance. The Edgetek XT product family includes a complete line of gen..