Thermal Properties Metric English Comments
Softening Point 42.0 - 48.0 °C
108 - 118 °F
Method R-003
Nitriflex S-6H Styrene Butadiene Copolymer
Applications: Copolymer with an ultra high level of combined styrene, aimed at compounds that require high hardness level, good resistance to abrasion, tearing and flection.Information provided by D..