Polymer Property : Softening Point = 117 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Softening Point 117 - 127 °C
243 - 261 °F
Beijing Ranger Chem SM-607R Solid Epoxy Resin
Information provided by Beijing Ranger Chemical Co.
Softening Point 117 °C
243 °F
Kofler Heating Stage
SK Chemicals SKYTHANE® 400 Hotmelt Grade UB Polyurethane
SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical pr..