Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Softening Point = 1190 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Softening Point 644 °C
1190 °F
Ferro CF 7574 Glaze and Sealant Glass
Glass Type: Zn-B-Si Typical Powder Form: VSD Typical Application: Pyrex Silicon Ferro's electronic and specialty glass group has produced over 3,000 formulations. Many are used as protective and ..
Softening Point 645 °C
1190 °F
Ferro EG 2807 Metal Sealing
Glass Type: Zn-B-Si (devit) Typical Powder Form: VSD Typical Application: Kovar Mo, W Ferro Metal Sealing glasses are formulated for sealing a wide range of metal packages and parts, including matc..
Softening Point 646 °C
1190 °F
Viscosity 10<sup>7.6</sup> dPa s; ISO 7884-3
Schott Glass 8516 Sealing Glass
Sealing glass for Fe-Ni alloys, high IR-absorbing, lead-free, of poor evaporation Reed switches The heavy metal content for the elements lead, cadmium, mercury, and hexavalent chromium is below 10..
Softening Point 645 °C
1190 °F
Corning 0159 Lead Barium Crushed/Powdered Glass
Available in mesh sizes 4 through 325 and can be customized. Used for sealing and other applications.Information provided by Corning Incorporated.
Softening Point 646 °C
1190 °F
Corning 9010 Alkali Barium Crushed Glass
Used for sealing and other applications.Information provided by Corning Incorporated.
Copyright © lookpolymers.com All Rights Reserved