Thermal Properties | Metric | English | Comments |
---|---|---|---|
Softening Point | 1200 °C | 2190 °F | |
BCC Products BC 37 Ceramic Microspheres BC 37 are hollow microspheres, which are ceramic in nature. They are an efficient lightweight filler material to be used in applications with most resins.Information provided by BCC Products, Inc. |