Thermal Properties | Metric | English | Comments |
---|---|---|---|
Softening Point | 704 °C | 1300 °F | |
Potters Industries Spheriglass® 1922 Solid Glass Spheres Description: Spheriglass® fine solid glass spheres are used as an additive for thermoplastic and thermosetting resin systems. Glass spheres give products many benefits such as:Low Uniform Shrinkage.. |
|||
Softening Point | 704 °C | 1300 °F | |
Potters Industries Spheriglass® 2024 Solid Glass Spheres Description: Spheriglass® fine solid glass spheres are used as an additive for thermoplastic and thermosetting resin systems. Glass spheres give products many benefits such as:Low Uniform Shrinkage.. |
|||
Softening Point | 704 °C | 1300 °F | |
Potters Industries Spheriglass® 2429 Solid Glass Spheres Description: Spheriglass® fine solid glass spheres are used as an additive for thermoplastic and thermosetting resin systems. Glass spheres give products many benefits such as:Low Uniform Shrinkage.. |
|||
Softening Point | 704 °C | 1300 °F | |
Potters Industries Spheriglass® 2530 Solid Glass Spheres Description: Spheriglass® fine solid glass spheres are used as an additive for thermoplastic and thermosetting resin systems. Glass spheres give products many benefits such as:Low Uniform Shrinkage.. |
|||
Softening Point | 704 °C | 1300 °F | |
Potters Industries Spheriglass® 3000 Solid Glass Spheres Description: Spheriglass® fine solid glass spheres are used as an additive for thermoplastic and thermosetting resin systems. Glass spheres give products many benefits such as:Low Uniform Shrinkage.. |
|||
Softening Point | 704 °C | 1300 °F | |
Potters Industries Spheriglass® 5000 Solid Glass Spheres Description: Spheriglass® fine solid glass spheres are used as an additive for thermoplastic and thermosetting resin systems. Glass spheres give products many benefits such as:Low Uniform Shrinkage.. |
|||
Softening Point | 702 °C | 1300 °F | |
Ferro F 2719 Metal Sealing Glass Type: Si-Ba Alkali Typical Powder Form: VSD Typical Application: Kovar Ferro Metal Sealing glasses are formulated for sealing a wide range of metal packages and parts, including matched seals.. |
|||
Softening Point | 705 °C | 1300 °F | Viscosity 10<sup>7.6</sup> dPa s; ISO 7884-3 |
Schott Glass 8270 Borosilicate Glass Borosilicate glass for sealing to Kovar metal and molybdenum, electrically highly insulating, defined UV absorption, stabilized against solarization Backlights The heavy metal content for the elem.. |
|||
Softening Point | 705 °C | 1300 °F | Viscosity 10<sup>7.6</sup> dPa s; ISO 7884-3 |
Schott Glass 8337B Borosilicate Glass Borosilicate glass for sealing to Kovar metal and tungsten, highly UV-transmitting photomultiplier and UV detectors The heavy metal content for the elements lead, cadmium, mercury, and hexavalent .. |