Polymer Property : Softening Point = 1340 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Softening Point 1340 °C
2440 °F
Temperature sample yields under load of push rod in CTE determination
Zircar Ceramics SALI-2 Alumina Insulation
SALI-2 is a premium grade rigid insulation board used as hotface insulation or a precision machined furnace fixtures.Information provided by Zircar Ceramics.