Thermal Properties | Metric | English | Comments |
---|---|---|---|
Softening Point | 1350 °C | 2460 °F | |
Corning Pyroceram® Glass Ceramic High strength, high elastic modulus, and uniform dielectric properties. Pyroceram® can be manufactured in ogival ( pointed arch) shapes, hemispheres, pressware sheets, and various machined shapes. .. |