Polymer Property : Softening Point = 193 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Softening Point 89.7 °C
193 °F
ETM based on ASTM D-6090-97; ETM E-24
ExxonMobil ESCOREZ™ 2173 (Europe) Petroleum Hydrocarbon Resin
ESCOREZ™ 2173 is a narrow molecular weight aromatic modified aliphatic resin giving excellent compatibility with natural and most synthetic rubbers and with EVA copolymers. It provides low viscosit..