Polymer Property : Softening Point = 205 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Softening Point 205 °C
401 °F
Valley Adhesives EM-221 Low Temperature Application Glue Stick
Valley Adhesives EM-221 Low Temperature Application Glue StickRapid strength build up to 0149; Excellent hot tack and wetting; Safe on styrofoam and heat sensitive materials; Bonds corrugated boxes ..