Thermal Properties Metric English Comments
Softening Point 1260 °C
2300 °F
Mid-Mountain Materials THERMOSEAL® 2000 High Temperature Cement
Description: A family of high temperature resistant cements carefully formulated to withstand thermal expansion and contraction under fluctuating heat conditions. THERMOSEAL® THERMAL CEMENTS are ..