Thermal Properties Metric English Comments
Softening Point 145 - 155 °C
293 - 311 °F
Oceanchem Group Brominated Epoxy Oligomers-3 (BEP-3)
Molecular Formula: (C36H32Br8O6)nCas No.: 68928-70-1Application: BEP-3 is a high molecular weight brominated epoxy polymeric flame retardant designed for a broad range of thermoplastic applications...
Softening Point 149 - 155 °C
300 - 311 °F
Average value: 149 °C Grade Count:14
Overview of materials for Cyanoacrylate Adhesive
This property data is a summary of similar materials in the MatWeb database for the category "Cyanoacrylate Adhesive". Each property range of values reported is minimum and maximum values of appropr..