Thermal Properties | Metric | English | Comments |
---|---|---|---|
Softening Point | 1710 °C | 3110 °F | Varies with thermal history |
Saint-Gobain Spectrosil® 1000 Optical Fused Quartz Spectrosil® 1000 grade is used for non-transmissive mirrors and substrates, and other high purity components which do not require specified optical transmission.Spectrosil® is a synthetic fuse.. |
|||
Softening Point | 1710 °C | 3110 °F | Varies with thermal history |
Saint-Gobain Spectrosil® 2000 Optical Fused Quartz Spectrosil® 2000 is a deep UV, fluorescence-free grade.Spectrosil® is a synthetic fused silica manufactured using a patented, environmentally friendly process that results in a virtually chlor.. |
|||
Softening Point | 1710 °C | 3110 °F | Varies with thermal history |
Saint-Gobain Spectrosil® 2100 Optical Fused Quartz Spectrosil® 2100 has improved refractive index homogeneity.Spectrosil® is a synthetic fused silica manufactured using a patented, environmentally friendly process that results in a virtually c.. |
|||
Softening Point | 1710 °C | 3110 °F | Varies with thermal history |
Saint-Gobain Spectrosil® 2200 Optical Fused Quartz Spectrosil® 2200 grade is an excimer laser grade developed for maximum transmission and prolonged life in microlithography and other critical deep UV applications using KrF (248 nm) and ArF (193 .. |