Thermal Properties | Metric | English | Comments |
---|---|---|---|
Softening Point | 466 °C | 871 °F | |
Ferro EG 4010 Display Device Glass Type: Pb-B-AL Typical Powder Form: VSD Typical Application: Dielectric Ferro's display sealing glasses and dielectrics are low-temperature lead glasses suitable for hermetic sealing and pas.. |