Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Softening Point = 55.0 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Softening Point 55.0 - 85.0 °C
131 - 185 °F
M Chemical GUARD DOGâ„¢ UV622 HALS Light Stabilizer
GUARD DOGâ„¢ UV662 is a solid, polymeric type, free radical scavenger hindered amine light stabilizer that is used to protect a wide range of polymers against degradation caused by exposure to UV..
Softening Point 55.0 - 60.0 °C
131 - 140 °F
MQSA 70 A
Lubrizol Advanced Materials PEARLBOND® 100 Linear Thermoplastic Polyurethane
Pearlbondâ„¢ 100 is a linear, polycaprolactone-based polyurethane, supplied in form of small white granules, which combines a very high crystallization rate with a very high thermoplasticity leve..
Softening Point 55.0 - 60.0 °C
131 - 140 °F
MQSA 70 A
Lubrizol Advanced Materials PEARLBOND® 106 Linear Thermoplastic Polyurethane
Pearlbondâ„¢ 106.is a linear, aromatic polyurethane, supplied in form of small white or slightly yellowish granules, which combines a high crystallisation rate with a very high thermoplasticity l..
Softening Point 55.0 - 60.0 °C
131 - 140 °F
Kolfer; MQSA 70 A
Lubrizol Advanced Materials PEARLBOND® 120 Linear Thermoplastic Polyurethane
Pearlbond® 120 is a linear, polycaprolactone-based polyurethane, supplied in form of small white granules, which combines an extremely high crystallization rate with a very high thermoplasticity ..
Softening Point 55.0 - 60.0 °C
131 - 140 °F
MQSA 70 A
Lubrizol Advanced Materials PEARLBOND® 121 Linear Thermoplastic Polyurethane
Pearlbondâ„¢ 121 is a linear, polycaprolactone-based polyurethane, supplied in form of small white granules, which combines an extremely high crystallization rate with a very high thermoplasticit..
Softening Point 55.0 - 60.0 °C
131 - 140 °F
MQSA 70 A
Lubrizol Advanced Materials PEARLBOND® 122 Linear Thermoplastic Polyurethane
Pearlbondâ„¢ 122 is a linear, polycaprolactone-based polyurethane, supplied in form of small white granules, which combines an extremely high crystallization rate with a very high thermoplasticit..
Softening Point 55.0 - 60.0 °C
131 - 140 °F
MQSA 70 A
Lubrizol Advanced Materials Pearlbond® 180 Thermoplastic Polyurethane
Pearlbondâ„¢ 180 is a linear, polyester-based polyurethane, supplied in form of small white granules, which combines a very high crystallization rate with a very high thermoplasticity level. It i..
Softening Point 55.0 - 60.0 °C
131 - 140 °F
MQSA 70 A
Lubrizol Advanced Materials PEARLBOND® 101 Linear Thermoplastic Polyurethane
Pearlbondâ„¢ 101 is a linear, polycaprolactone-based polyurethane, supplied in form of small white granules, which combines a very high crystallization rate with a very high thermoplasticity leve..
Softening Point 55.0 - 60.0 °C
131 - 140 °F
MQSA 70 A
Lubrizol Advanced Materials PEARLBOND® 123 Linear Thermoplastic Polyurethane
Pearlbondâ„¢ 123 is a linear, polycaprolactone-based polyurethane, supplied in form of small white granules, which combines an extremely high crystallization rate with a very high thermoplasticit..
Softening Point 55.0 - 60.0 °C
131 - 140 °F
Aquabond Technologies Aquabond™ ABS-65 Water Soluble Adhesive and Bonding Thermoplastic
Description: Aquabond's water soluble thermoplastic is designed for temporary mounting of hard materials for slicing, dicing, grinding, lapping and polishing and comes in 3 different bonding tem..
Softening Point 55.0 - 60.0 °C
131 - 140 °F
MQSA 70 A
Lubrizol Advanced Materials PEARLBOND® 103 Linear Thermoplastic Polyurethane
Pearlbond™ 103 is a linear, polycaprolactone-based polyurethane, supplied in form of small white granules, which combines a very high crystallization rate with a very high thermoplasticity level. I..
Copyright © lookpolymers.com All Rights Reserved