Polymer Property : Softening Point = 66.0 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Softening Point 54.0 - 66.0 °C
129 - 151 °F
flow beginning
Taiwan Sheen Soon Sheenthane® AH-640 TPU for Hotmelt Adhesive
Thermoplastic polyurethane elastomer for hard hotmelt adhesiveExcellent bonding strength for polyester, TPU, nylon, PVC, leather, fabrics, etc. Melt flow may be customized. Used for hot melt adhes..
Softening Point 54.0 - 66.0 °C
129 - 151 °F
flow beginning
Taiwan Sheen Soon Sheenthane® AH-650 TPU for Hotmelt Adhesive
Thermoplastic polyurethane elastomer for hard hotmelt adhesiveExcellent bonding strength for polyester, TPU, nylon, PVC, leather, fabrics, etc. Melt flow may be customized. Used for hot melt adhes..
Softening Point 54.0 - 66.0 °C
129 - 151 °F
flow beginning
Taiwan Sheen Soon Sheenthane® AH-810 TPU for Hotmelt Adhesive
Thermoplastic polyurethane elastomer for hotmelt adhesiveNon-yellowing, aliphatic gradeExcellent bonding strength for polyester, TPU, nylon, PVC, leather, fabrics, etc. Melt flow may be customized...