Thermal Properties Metric English Comments
Softening Point 372 °C
702 °F
Ferro CF 7583 Low-Temperature Sealing
DEVITRIFYING Typical Powder Form: TF Ferro's line of low-temperature sealing glasses are comprised of lead-borate (vitreous) and lead-zinc-borate crystallizing glasses formulated to meet specific t..