Thermal Properties | Metric | English | Comments |
---|---|---|---|
Softening Point | 750 °C | 1380 °F | |
Ferro EG 0024 Specialty Glass Glass Type: Si-B-MG-Al Typical Powder Form: VWG Typical Application: Sintering Aid Ferro offers a wide range of compositions for specialty applications including sintering aids used in the glass-ph.. |