Polymer Property : Softening Point = 840 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Softening Point 840 - 850 °C
1540 - 1560 °F
Mo-Sci Corporation GL-0271 E-Glass Spheres
Appearance: Solid low alkali E-glass beads with greenish color.Chemical Durability: Weight loss @ 90°C for 24 hrs in 5% HCl 0.3 mg/cm2Information provided by Mo-Sci Corporation.