Polymer Property : Softening Point = 915.0 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Softening Point 915.0 °C
1679 °F
Viscosity 10<sup>7.6</sup> dPa s; ISO 7884-3
Schott Glass 8230 Intermediate sealing glass
The heavy metal content for the elements lead, cadmium, mercury, and hexavalent chromium is below 100 ppmInformation provided by SCHOTT AG.