Thermal Properties Metric English Comments
Softening Point 500 °C
932 °F
Dilatometric
Mo-Sci Corporation WB-40-N White B Filter Glass
Applications: Lead-free NVIS White class B filter glass for white LED sources.Information provided by Mo-Sci Corporation.
Softening Point 500 °C
932 °F
Saint-Gobain Micaver® Glass-Mica Electrical Insulator, Compression Moldings
Glass-mica compound that occupies a place between plastics and ceramics in terms of usage temperature. It can be molded and machined like plastics and has the mechanical properties (strength, hardn..
Softening Point 500 °C
932 °F
Permanent Softening
CMW® 28 Copper Alloy
CMW® 28 material is a copper base alloy having very high electrical and thermal conductivity and medium strength and toughness. It is a heat treatable alloy and develops its strength and hardness t..
Softening Point 500 °C
932 °F
Permanent Softening
CMW® 3 Copper Alloy
CMW® 3 material is a high strength, high conductivity copper base alloy. CMW® 3 material is heat treatable. Optimum mechanical and physical properties of CMW® 3 material are developed by heat tre..
Softening Point 500 °C
932 °F
Dilatometric
Mo-Sci Corporation YB-40-N Yellow B Filter Glass
Applications: Lead-free NVIS Yellow class B filter glass for white LED sources.Information provided by Mo-Sci Corporation.