Polymer Property : Softening Point = 950 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Softening Point 950 °C
1740 °F
Dilatometric @ 10psi
Zircar Zirconia ZYC Zirconia Cylinders Insulation
Zircar Zirconia Cylinders Type ZYC are rigid, free standing refractory structures composed of yttria stabilized zirconia fibers that are bonded with silica. The material is evenly bonded, allowing ..
Softening Point 950 °C
1740 °F
Dilatometric @ 10psi
Zircar Zirconia ZYC Zirconia Cylinders Insulation
Zircar Zirconia Cylinders Type ZYC are rigid, free standing refractory structures composed of yttria stabilized zirconia fibers that are bonded with silica. The material is evenly bonded, allowing ..