Thermal Properties | Metric | English | Comments |
---|---|---|---|
Boiling Point | >= 190 °C @Pressure 0.000667 MPa |
>= 374 °F @Pressure 0.0967 psi |
|
BASF Lupranate® 223 Isocyanate Description: Lupranate® 223 Isocyanate is a low viscosity derivative of both pure-MDI and polymeric-MDI. With a functionality of approximately 2.2, this isocyanate can be formulated into applicatio.. |
|||
Boiling Point | >= 190 °C @Pressure 0.000667 MPa |
>= 374 °F @Pressure 0.0967 psi |
|
BASF Lupranate® 230 Isocyanate Description: Lupranate® 230 Isocyanate is a low viscosity derivative of both pure-MDI and polymeric-MDI. With a functionality of approximately 2.2, this isocyanate can be formulated into applicatio.. |
|||
Boiling Point | >= 190 °C @Pressure 0.000667 MPa |
>= 374 °F @Pressure 0.0967 psi |
|
BASF Lupranate® 245 Isocyanate Description: Lupranate® 245 Isocyanate is a low viscosity polymeric diphenylmethane diisocyanate (polymeric MDI) containing a very high amount of monomeric diphenylmethane diisocyanate (pure MDI)In.. |
|||
Boiling Point | >= 190 °C @Pressure 0.000667 MPa |
>= 374 °F @Pressure 0.0967 psi |
|
BASF Lupranate® 273 Isocyanate Description: Lupranate® 273 Isocyanate is a solvent-free polymeric MDI with a functionality of approximately 2.3. Lupranate® 273 Isocyanate is a polymeric MDI which contains a relatively high leve.. |
|||
Boiling Point | >= 190 °C @Pressure 0.000667 MPa |
>= 374 °F @Pressure 0.0967 psi |
|
BASF Lupranate® 279 Isocyanate Description: Lupranate® 279 Isocyanate is a 14% free-NCO prepolymer based on monomeric MDI chemistry. Lupranate 279 Isocyanate provides the lengthened open-time and high elongation desired in appli.. |
|||
Boiling Point | >= 190 °C @Pressure 0.000667 MPa |
>= 374 °F @Pressure 0.0967 psi |
|
BASF Lupranate® 5020 Isocyanate Description: Lupranate® 5020 Isocyanate is a low free-NCO prepolymer based on pure MDI. The 9.5% free-NCO of Lupranate® 5020 Isocyanate lends itself to one-component applications, such as but not .. |
|||
Boiling Point | >= 190 °C @Pressure 0.000667 MPa |
>= 374 °F @Pressure 0.0967 psi |
|
BASF Lupranate® 5030 Isocyanate Description: Lupranate® 5030 Isocyanate is a liquid urethane modified diphenylmethane diisocyanate. Lupranate 5030 Isocyanate is used in conjunction with high molecular weight polyester or polyethe.. |
|||
Boiling Point | >= 190 °C @Pressure 0.000667 MPa |
>= 374 °F @Pressure 0.0967 psi |
|
BASF Lupranate® 5050 Isocyanate Description: Lupranate® 5050 Isocyanate is a prepolymer based on a modified, pure MDI. The intermediate free-NCO and slightly enhanced functionality of Lupranate 5050 isocyanate has benefited the f.. |
|||
Boiling Point | >= 190 °C @Pressure 0.000667 MPa |
>= 374 °F @Pressure 0.0967 psi |
|
BASF Lupranate® 5090 Isocyanate Description: Lupranate® 5090 Isocyanate is a liquid prepolymer of pure, diphenylmethane diisocyanate (MDI). The Lupranate 5090 Isocyanate has been formulated for improved low-temperature stability .. |
|||
Boiling Point | >= 190 °C @Pressure 0.000667 MPa |
>= 374 °F @Pressure 0.0967 psi |
|
BASF Lupranate® 5110 Isocyanate Description: Lupranate® 5110 is a stable liquid polymeric MDI prepolymer. When used in molded flexible foams, Lupranate® 5110 Isocyanate demonstrates the ability to combine softness of foam with g.. |
|||
Boiling Point | >= 190 °C @Pressure 0.000667 MPa |
>= 374 °F @Pressure 0.0967 psi |
|
BASF Lupranate® 5140 Isocyanate Description: Lupranate® 5140 Isocyanate is a prepolymer based on a modified, pure MDI. The intermediate free-NCO and enhanced functionality of Lupranate 5140 isocyanate has benefited the formulatio.. |
|||
Boiling Point | >= 190 °C @Pressure 0.000667 MPa |
>= 374 °F @Pressure 0.0967 psi |
|
BASF Lupranate® MT Isocyanate Description: Lupranate® MT Isocyanate, a solid at room temperature, is essentially pure 4,4´-diphenylmethane diisocyanate, having a functionality of 2.0. Lupranate® MT Isocyanate is used in the .. |
|||
Boiling Point | >= 190 °C @Pressure 0.000667 MPa |
>= 374 °F @Pressure 0.0967 psi |
|
BASF Lupranate® R2500 Isocyanate Description: Lupranate® R2500 Isocyanate is a polymeric MDI with a functionality of approximately 2.7. Careful control of the MDI distribution in Lupranate R2500 Isocyanate helps provide uniform re.. |
|||
Boiling Point | >= 190 °C @Pressure 0.000667 MPa |
>= 374 °F @Pressure 0.0967 psi |
|
BASF Lupranate® 241 Isocyanate Description: Lupranate® 241 Isocyanate is a low functionality (approximately 2.3) low viscosity polymeric MDI with high2,4’-MDI isomer content. Lupranate® 241 Isocyanate exhibits excellent low t.. |
|||
Boiling Point | >= 190 °C @Pressure 0.000667 MPa |
>= 374 °F @Pressure 0.0967 psi |
|
BASF Lupranate® 259 Isocyanate Description: Lupranate® 259 Isocyanate is a modified pure MDI. No 259 Isocyanate is applicable for use in all CASE applications.Information provided by BASF |
|||
Boiling Point | >= 190 °C @Pressure 0.000667 MPa |
>= 374 °F @Pressure 0.0967 psi |
|
BASF Lupranate® 266 Isocyanate Description: Lupranate® 266 Isocyanate is a low viscosity polymeric MDI containing a high amount of 2,4’ diphenylmethane diisocyanate. Lupranate® 266 Isocyanate displays excellent low temperatur.. |
|||
Boiling Point | >= 190 °C @Pressure 0.000667 MPa |
>= 374 °F @Pressure 0.0967 psi |
|
BASF Lupranate® 274 Isocyanate Description: Lupranate® 274 Isocyanate is a polymeric MDI with a functionality of approximately 2.7. Lupranate 274 Isocyanate is suitable for the production of rigid insulation foams by molding, sp.. |
|||
Boiling Point | >= 190 °C @Pressure 0.000667 MPa |
>= 374 °F @Pressure 0.0967 psi |
|
BASF Lupranate® 275 Isocyanate Description: Lupranate® 275 Isocyanate is a 15.9% Free-NCO prepolymer based on diphenylmethane diisocyanate (MDI) chemistry. The formulation of Lupranate 275 Isocyanate provides the low viscosity a.. |
|||
Boiling Point | >= 190 °C @Pressure 0.000667 MPa |
>= 374 °F @Pressure 0.0967 psi |
|
BASF Lupranate® 5060 Isocyanate Description: Lupranate® 5060 Isocyanate is a low functional prepolymer based on monomeric MDI. Lupranate® 5060 isocyanate is suitable for use in a broad range of flexible, semi-flexible, and cast .. |
|||
Boiling Point | >= 190 °C @Pressure 0.000667 MPa |
>= 374 °F @Pressure 0.0967 psi |
|
BASF Lupranate® 5130 Isocyanate Description: Lupranate® 5130 Isocyanate has the combined characteristics of a liquid carbodiimidemodified isocyanate and a pure MDI prepolymer. The relatively low functionality and high free-NCO of.. |
|||
Boiling Point | >= 190 °C @Pressure 0.000667 MPa |
>= 374 °F @Pressure 0.0967 psi |
|
BASF Lupranate® 5220 Isocyanate Description: Lupranate® 5220 Isocyanate is a low viscosity polymeric MDI containing a high amount of diphenylmethane diisocyanate (monomeric MDI).Information provided by BASF |
|||
Boiling Point | >= 190 °C @Pressure 0.000667 MPa |
>= 374 °F @Pressure 0.0967 psi |
|
BASF Lupranate® 78 Isocyanate Description: Lupranate® 78 Isocyanate is a polymeric MDI with a functionality of approximately 2.3. This product exhibits excellent low temperature stability. Lupranate 78 Isocyanate will remain a .. |
|||
Boiling Point | >= 190 °C @Pressure 0.000667 MPa |
>= 374 °F @Pressure 0.0967 psi |
|
BASF Lupranate® 81 Isocyanate Description: Lupranate® 81 Isocyanate is a carbodiimide modified pure MDI with a higher 2,4’-isomer content and a functionality of approximately 2.1. Lupranate 81 Isocyanate exhibits good low temp.. |
|||
Boiling Point | >= 190 °C @Pressure 0.000667 MPa |
>= 374 °F @Pressure 0.0967 psi |
|
BASF Lupranate® LP30D Isocyanate Description: Lupranate® LP30D isocyanate is a solvent-free, modified pure diphenylmethane diisocyanate which is liquid at 30°C. It is designed to replace pure MDI in applications where it is desir.. |
|||
Boiling Point | >= 190 °C @Pressure 0.000667 MPa |
>= 374 °F @Pressure 0.0967 psi |
|
BASF Lupranate® M Isocyanate Description: Lupranate® M Isocyanate, a solid at room temperature, is essentially pure 4,4´-diphenylmethane diisocyanate, having a functionality of 2.0. Lupranate M Isocyanate is used in the isoc.. |
|||
Boiling Point | >= 190 °C @Pressure 0.000667 MPa |
>= 374 °F @Pressure 0.0967 psi |
|
BASF Lupranate® M20FB Isocyanate Description: Lupranate® M20FB is a polymeric MDI with a functionality of approximately 2.7. Lupranate® M20FB has faster reactivity than polymeric MDI currently used in the wood panel industry. Thi.. |
|||
Boiling Point | >= 190 °C @Pressure 0.000667 MPa |
>= 374 °F @Pressure 0.0967 psi |
|
BASF Lupranate® MP102 Isocyanate Modified MDI Description: Lupranate® MP102 Isocyanate is a liquid, modified short chain prepolymer based on pure 4,4’-diphenylmethane diisocyanate (MDI). Lupranate MP102 Isocyanate is used in conjunction with .. |
|||
Boiling Point | >= 190 °C @Pressure 0.000667 MPa |
>= 374 °F @Pressure 0.0967 psi |
|
BASF Lupranate® LP30 Isocyanate Description: Lupranate® LP30 isocyanate is a solvent-free, modified pure diphenylmethane diisocyanate which is liquid at 30°C. It is designed to replace pure MDI in applications where it is desira.. |
|||
Boiling Point | >= 190 °C @Pressure 0.000667 MPa |
>= 374 °F @Pressure 0.0967 psi |
|
BASF Lupranate® M10 Isocyanate Description: Lupranate® M10 Isocyanate is a solvent-free polymeric MDI with a functionality of approximately 2.3. Lupranate M10 Isocyanate is a polymeric MDI which contains a relatively high level .. |
|||
Boiling Point | >= 190 °C @Pressure 0.000667 MPa |
>= 374 °F @Pressure 0.0967 psi |
|
BASF Lupranate® M20 Isocyanate Description: Lupranate® M20 Isocyanate is a polymeric MDI with a functionality of approximately 2.7. Lupranate M20 Isocyanate can be used for the production of rigid insulation foams by molding, sp.. |