Thermal Properties | Metric | English | Comments |
---|---|---|---|
Boiling Point | 82.2 °C | 180 °F | Initial; ASTM D86 |
ExxonMobil Exxsol™ DSP 75-95 Dearomatized Fluid Availability: South America Appearance: Clear/Transparent LiquidInformation provided by ExxonMobil |
|||
Boiling Point | 82.2 °C | 180 °F | Initial; ASTM 1078 |
ExxonMobil Exxsol™ DSP 80/100 TH Dearomatized Fluid Availability: Asia Pacific Appearance: Clear/Transparent LiquidInformation provided by ExxonMobil |
|||
Boiling Point | 82.2 °C | 180 °F | Initial; ASTM D1078 |
ExxonMobil IPA Isopropyl Alcohol Appearance: Clear/Transparent LiquidAvailability: Africa & Middle East, Europe, Asia Pacific, Central America, North America and South AmericaInformation provided by ExxonMobil |