Polymer Property : Boiling Point = 102 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Boiling Point 102 °C
216 °F
Permabond CleanerA Surface Cleaner
Permabond Cleaner A is a general purpose industrial cleaner for cleaning and degreasing surfaces prior to bonding with any Permabond adhesive. Where surfaces are greasy or dirty, wiping with CLEANER..
Boiling Point 102 °C
216 °F
Permabond CSA Cyanoacrylate Surface Activator
Permabond C Surface Activator (CSA) is used in conjunction with Permabond cyanoacrylate adhesives to promote a faster cure and to extend their gap-filling capabilities. It also enables fillets of cu..
Boiling Point 102 °C
216 °F
Solvay MIRANOL® JS CONC Surfactant
Description: Amphoteric detergent, good wetting agent. Stable in highly acidic and alkali media. No compliant with the EU's detergent biodegradability regulation.Identification: SODIUM CAPRYLOAMPHO..
Boiling Point 102 - 105 °C
216 - 221 °F
BASF 2-Methyl-3-butyn-2-ol
Formula: C5H8OCAS: 115-19-5Description: 2-Methyl-3-butyn-2-ol is a colorless to yellow liquid, with an alcohol-like odor. It is miscible in waterSynonyms: 2-Methyl-3-butin-2-ol, 2-Methylbut-3-in-2-..