Thermal Properties | Metric | English | Comments |
---|---|---|---|
Boiling Point | 41.0 °C @Pressure 0.1013 MPa |
106 °F @Pressure 14.69 psi |
|
Shandong Dongyue Shenzhou New Material Co Tetrafluoroethane Β-sultone Conformable with: Q/DYS 008-2007TFE Beta-sultone is a colorless transparent liquid. Industrial produced TFE Beta-sultone is mixture of ringlike and straight chain structure, and ringlike structure .. |
|||
Boiling Point | 41.3 °C | 106 °F | |
Dow Corning Z-1218 METHYLDICHLOROSILANE Methyldichlorosilane fluidInformation provided by Dow Corning |
|||
Boiling Point | 41.0 °C | 106 °F | |
3M Novec™ 71DE Engineered Fluid 3M™ Novec™ 71DE is an azeotrope containing 3M™ Novec™ 7100 and 1,2 trans-dichloroethylene. It maintains a constant liquid and vapor composition at its boiling point. It can be used in many mediu.. |