Polymer Property : Boiling Point = 110 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Boiling Point 110 °C
230 °F
Solvay Chemicals CASO® TEC SOLUTION 25-29% Calcium Chloride
CASO® Calcium Chloride technical grade can be used in various applications in industrial, public and private sectors.REACH Registration Number: 01-2119494219-28/ CAS number: 10043-52-4/ EINECS - ..
Boiling Point 110 °C
230 °F
Solvay Specialty Polymers Galden® SV110 PFPE Solvent
Galden® SV grades are specifically recommended for use as solvents.Galden® PFPE is a line of high-performance, inert, fluorinated fluids. Various grades, with a variety of service temperature..
Boiling Point 110 °C
230 °F
Solvay Specialty Polymers Galden® HT110 PFPE Heat Transfer Fluid
Galden® HT grades are specifically recommended for use as heat transfer fluids.Galden® PFPE is a line of high-performance, inert, fluorinated fluids. Various grades, with a variety of service tem..
Boiling Point 110 °C
230 °F
BASF Dipropylamine
Formula: C6H