Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Boiling Point = 2.30 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Boiling Point -16.5 °C
2.30 °F
Solvay Chemicals SOLKANE® 227 ea technical grade
HFC SOLKANE® 227ea technical grade is used in air conditioning units where elevated ambient temperatures are present. CAS-No.: 431-89-0 / EC-No.: 207-079-2 Uses: Refrigerant and Foaming agentInfo..
Boiling Point -16.5 °C
2.30 °F
Solvay Chemicals SOLKANE® 227 pharma
SOLKANE® 227 pharma is also known as HFA 227, HFC 227 or 1,1,1,2,3,3,3-heptafluoropropane. CAS-No.: 431-89-0 / EC-No.: 207-079-2 Uses: PropellantInformation provided by Solvay
Boiling Point -16.5 °C
2.30 °F
Solvay Chemicals SOLKAFLAM® 227 UL
SOLKAFLAM® 227 UL - recognized component fire extinguishing agents CAS-No.: 431-89-0 / EC-No.: 207-079-2 Uses: Fire extinguishing agentInformation provided by Solvay