Thermal Properties | Metric | English | Comments |
---|---|---|---|
Boiling Point | 93.9 °C | 201 °F | Initial; ASTM D86 |
ExxonMobil Exxsol™ Heptane Dearomatized Fluid Availability: Africa & Middle East, Asia Pacific, Europe, Central America, North America and South AmericaAppearance: Clear/Transparent LiquidInformation provided by ExxonMobil |
|||
Boiling Point | 94.0 °C | 201 °F | |
BASF N-Butyl Vinyl Ether Formula: C6H12OCAS: 11-34-2Description: N-Butyl vinyl ether is a colorless to yellow liquid, with an ether-like odor. It is sparingly soluble in water.Synonyms: NBVE, 1-(Vinyloxy)butane, 1-(Ethenyl.. |