Thermal Properties Metric English Comments
Boiling Point 111 °C
232 °F
LG Chemical Toluene
Colorless liquid with benzene odor, Heavier than air and highly inflammable, and Not soluble to water, Readily soluble in alcohol and etherStructure & Characteristics: C6H5CH3. Synthesized by extrac..
Boiling Point 111 - 114 °C
232 - 237 °F
BASF Lupragen® N 105 N-Methylmorpholine
Formula: C5H11NOCAS: 109-02-4Description: Lupragen® N 105 is a colorless to yellow liquid with an amine-like odor. It is miscible in water.Synonyms: N-Methyl-tetrahydro-1,4-oxazin, N-Methylmorphol..