Thermal Properties Metric English Comments
Boiling Point 113 - 116 °C
235 - 241 °F
BASF Vinyl Caprolactam
Formula: C8H13NOCAS: 2235-00-9Description: Vinyl caprolactam is a yellowish solid, with a faint specific odor. It is soluble in water.Synonyms: NVC, Vinyl-caprolactameApplications: Intermediate use..