Thermal Properties | Metric | English | Comments |
---|---|---|---|
Boiling Point | 268 °C | 514 °F | |
BASF 2-Methyl Imidazole Flake Formula: C4H6N2CAS: 693-98-1Description: 2-Methylimidazole or 2MI is a colorless to yellowish solid with an amine-like odor. Synonyms: 2-Methyl-1H-imidazoleApplications: Intermediate used in Pharmac.. |
|||
Boiling Point | 268 °C | 514 °F | |
BASF 2-Methyl Imidazole Pure Formula: C4H6N2CAS: 693-98-1Description: 2-Methylimidazole or 2MI is a colorless to yellowish solid with an amine-like odor. Synonyms: 2-Methyl-1H-imidazolApplications: Intermediate used in Pharmac.. |
|||
Boiling Point | 268 - 270 °C | 514 - 518 °F | |
BASF 2-Ethyl Imidazole Formula: C5H8N2CAS: 1072-62-4Description: 2-Ethyl Imidazole is a colorless to yellowish solid with an amine-like odor.Synonyms: 2EIApplications: It is used as a Pharmaceuticals, Crop protection agen.. |