Thermal Properties Metric English Comments
Boiling Point 333 °C
631 °F
atmospheric boiling point, 10% fraction; ASTM D1160
Paratherm Corporation Paratherm™ OR Heat Transfer Fluid
Description: Paratherm OR® is a sludge-resistant heat transfer fluid that combines substantial oxidation resistance with excellent thermal efficiency, high flash and fire points and extended servic..