Thermal Properties Metric English Comments
Boiling Point 3360 °C
6080 °F
American Elements Cerium Nanoparticles
General DescriptionCerium (Ce) Nanoparticles, nanodots or nanopowder are black spherical high surface area particles. Nanoscale Cerium Particles are typically 5 - 40 nanometers (nm) with specific su..