Polymer Property : Boiling Point = 554 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Boiling Point 166 - 290 °C
331 - 554 °F
LG Chemical C9 Product
Physical Properties: Colorless liquid similar to DIESEL oilObtained as a by-product from pyrolysis oil hydration plant which was produced from naphtha pyrolysis process. It is composed of hydrocarbo..